Skip to main content
. 2017 Jun 15;10(6):655. doi: 10.3390/ma10060655

Figure 6.

Figure 6

The permittivity of as-received and annealed SiBCN-Si3N4 ceramics at different temperatures: (a) the real part; (b) the imaginary part; and (c) tangent loss.