Figure 2.

Figure 2

Thermal characterization of component and alternating block copolymer ELPs. A) The hydrophilic (ELP-Scomp) and hydrophobic (ELP-Vcomp) component ELPs exhibited Tts that differed by 60–85°C. Homogeneous mixture of the components in ELP-SVB1 resulted in a Tt that was dominated by the hydrophobic component. B) Increasing the block size decreased the Tt across concentrations of 5–100 µM. Squares–experimental values; lines–logarithmic fit to experimental data.