Table 2.
The EC‐free superconcentrated electrolytes that could enable the successful intercalation of lithium ions into the graphite electrodes. The concentration listed in this table is in molarity (mol L–1)
Solvent | Lithium Salt | Successful Concentration | Reference |
---|---|---|---|
PC | LiBETI [LiN(SO2C2F5)2] | 2.72 m | Jeong et al.24 |
PC | LiPF6 | 3.0 m | Nie et al.[[qv: 11a]] |
PC | LiPF6 | 3.0 m | Ding et al.82 |
PC | LiClO4 | 3.8 m | Kim et al.83 |
DME | LiFSI (LiN(SO2F)2) | 3.6 m | Yamada et al.84 |
AN | LiTFSI (LiN(SO2CF3)2) | 4.5 m | Yamada et al.[[qv: 11b]] |
DMSO | LiTFSI (LiN(SO2CF3)2) | 3.2 m | Yamada et al.[[qv: 12a]] |
SL | LiTFSI (LiN(SO2CF3)2) | 3.0 m | Yamada et al.[[qv: 12a]] |
THF | LiTFSI (LiN(SO2CF3)2) | 3.0 m | Yamada et al.[[qv: 12a]] |
EA | LiPF6 + LiFSI | 0.5 m LiPF6 + 5 m LiFSI | Petibon et al.85 |