Skip to main content
. 2017 Aug 10;2017:1207208. doi: 10.1155/2017/1207208

Table 3.

Distribution of failure modes after shear bond strength testing (n = 16/group; BAC: benzalkonium chloride).

Adhesive system
Dentin
Cohesive failures in dentin (%) Adhesive failures at dentin/adhesive interface (%) Mixed failures (%)
After 24-hour storage

Adper Scotchbond 1XT without 1% BAC  
 Normal dentin 12.5 62.5 25
Adper Scotchbond 1XT without 1% BAC  
 Artificially eroded dentin 0 100 0
Adper Scotchbond 1XT with 1% BAC  
 Normal dentin 0 87.5 12.5
Adper Scotchbond 1XT with 1% BAC  
 Artificially eroded dentin 0 87.5 12.5
OptiBond FL without 1% BAC  
 Normal dentin 6.25 75 18.75
OptiBond FL without 1% BAC  
 Artificially eroded dentin 0 100 0
OptiBond FL with 1% BAC  
 Normal dentin 6.25 87.5 6.25
OptiBond FL with 1% BAC  
 Artificially eroded dentin 0 100 0

After 1-year storage

Adper Scotchbond 1XT without 1% BAC  
 Normal dentin 6.25 75 18.75
Adper Scotchbond 1XT without 1% BAC  
 Artificially eroded dentin 0 100 0
Adper Scotchbond 1XT with 1% BAC  
 Normal dentin 6.25 93.75 0
Adper Scotchbond 1XT with 1% BAC  
 Artificially eroded dentin 0 100 0
OptiBond FL without 1% BAC  
 Normal dentin 0 81.25 18.75
OptiBond FL without 1% BAC  
 Artificially eroded dentin 0 100 0
OptiBond FL with 1% BAC  
 Normal dentin 0 93.75 6.25
OptiBond FL with 1% BAC  
 Artificially eroded dentin 0 100 0