Spinal Implant RF‐Radiation‐Induced Heating (7 T) 3D‐FSE (15 min)
Material Length (cm) Weight (g) Implant (Δ°C) CTRL‐l (Δ°C) Diff‐1 (°C) CTRL‐2 (Δ°C) Diff‐2 (°C)
Rod
Pure titanium 5 5.5 0.8 0.4 0.4 0.4 0.4
10 10.8 0.9 1.1 −0.2 0.6 0.3
15 16.2 0.8 1.0 −0.2 0.8 0
20 21.6 0.9 0.9 0 0.7 0.2
20, cross‐linked 66.0 1.0 0.9 0.1 0.5 0.5
Titanium alloy 5 5.3 0.7 0.7 0 0.7 0
10 10.6 0.8 0.9 −0.1 1.1 −0.3
15 15.9 0.9 0.9 0 0.6 0.3
20 21.1 0.7 0.9 −0.2 0.7 0
20, cross‐linked 65.0 0.8 0.6 0.2 0.7 0.1
Cobalt–chrome 5 9.9 0.8 0.8 0 0.4 0.4
10 19.9 0.9 0.3 0.6 0.6 0.3
15 29.8 0.9 0.3 0.6 0.8 0.1
20 39.9 0.8 0.5 0.3 0.5 0.3
20, cross‐linked 102.6 0.8 0.6 0.2 0.6 0.2
Range (median) 5–20 (12.5) 5.5–102.6 (19.9) 0.7–1.0 (0.8) 0.3–1.1 (0.8) −0.2 to 0.6 (0) 0.4–1.1 (0.6) −0.3 to 0.5 (0.2)
Screw
Titanium alloy/cobalt–chrome 5.8 12.1 0.7 1.0 −0.3 0.5 0.2
Cross‐linking bridge
Titanium alloy 5.2 11.4 0.5 0.7 −0.2 0.5 0