Figure 1.

Figure 1

Output optical power evolution as the thickness of the thin film increases. The bottom axis shows the deposition time while the top axis represent the expected coating thickness at that moment. Several resonances can be distinguished. In the first order LMR observed, two components can be appreciated, corresponding each to a different mode.