Table 1.
The full width at half height (FWHH) and the crosslinking density of the different networks decreases as a function of different nanogel mass fraction.
| Formulation | FWHH (°C) | Rubbery Modulus (MPa); Tg + 40 °C |
|---|---|---|
| E9 | 54.2 ± 2.0 | 23.9 ± 3.9 |
| E9NG-5 | 47.4 ± 2.2 | 15.3 ± 1.4 |
| E9NG-10 | 47.1 ± 1.0 | 13.7± 1.8 |
| E9NG-20 | 32.8 ± 3.4 | 10.5 ± 0.5 |
| E9NG-30 | 26.5 ± 1.0 | 7.5 ± 0.5 |