. 2017 May 18;96(10):1122–1128. doi: 10.1177/0022034517709738

Figure 2.

Figure 2.

Pearson correlation between the percentage increase of crystal size and SDF concentrations. (A) The correlation between percentage increase of width of crystal and SDF concentration (coefficient R2 = 0.95, slope m = 2.20). (B) The correlation between percentage increase of length of crystal and SDF concentration (coefficient R2 = 0.90, slope m = 0.91). SDF, silver diamine fluoride.