Skip to main content
. 2017 Sep 7;7:10919. doi: 10.1038/s41598-017-11279-w

Figure 3.

Figure 3

(a,b) The hysteresis loop of MNPs with d = 150–350 nm and l = 200 nm and 500 nm, respectively. (c,d) The low field magnetic susceptibility (χ) and magnetization Mr/Ms was obtained as a function of MNP d = 150–350 nm and l = 50–500 nm for both single vortex state (dashed lines) and triple vortex state (solid lines). (e) The force exerted by MNPs with respect to applied magnetic field for d = 150–350 nm and l = 50–500 nm. (f) The comparison of cell viability of HeLa cells after magneto-mechanical cell destruction treatment using MNPs with d = 150–350 nm and l = 500 nm.