Skip to main content
. Author manuscript; available in PMC: 2018 Apr 1.
Published in final edited form as: J Biomater Sci Polym Ed. 2017 Feb 5;28(6):532–554. doi: 10.1080/09205063.2017.1286184

Figure 6.

Figure 6

Fiber diameter measurements (a) and apparent viscosity (b) of PPF-HA solutions (containing 1.25, 2.5, 5 and 10 wt% HA) printed at varied temperature, pressure (0.4 bar for 1.25 wt%, 0.5 bar for 2.5, 5, and 10 wt%), and speed to print fibers with similar diameters. Printing solutions extruded with a 0.840 mm (inner diameter) syringe tip. Measurements reported as mean ± standard deviation (n = 3).