Table 4.

Mean diameters of PVDF nanofibers with different feeding rates measured from SEM micrographs

Sample Solvent Concentration (w/v%) Voltage (kV) Distance (cm) Feeding rate (ml/h) Collector speed (rpm) Mean nanofiber diameter (nm)
S10 DMAC/acetone 30 15 18 0.3 1000 365.6 ± 13
S11 DMAC/acetone 30 15 18 0.5 1000 520.6 ± 14
S8 DMAC/acetone 30 15 18 0.7 1000 432.2 ± 21