X-ray diffraction data showing the crystallinity of prepared graphite oxide samples under different oxidation time, and exfoliation properties of GO in canola protein matrix after adhesive preparation. CPI–Canola protein isolate, GO-A, GO-B and GO-C–starting graphite oxide samples prepared by oxidizing graphite for 0.5 h, 2 h, and 4 h respectively. CPA GO-A, CPA GO-B and CPA GO-C are prepared by exfoliating 1% w/w (GO/protein) GO-A, GO-B and GO-C respectively in 10% w/v canola protein dispersion.