Fig. 1.

Fig. 1

(A) Material layout during molding of PUMA chip. 1: PDMS mold; 2: PUMA resin; 3: PTFE posts; 4: polypropylene sheet; 5: cellophane (or Aclar). (B) Two methods of interfacing PUMA chip with external tubing: 1: PUMA chip; 2: barb elbow connector; 3: polyurethane tubing; 4: additional resin to seal leak (Dymax 186M); 5: PTFE tubing; 6: polyolefin heat-shrink; 7: retaining ring.