Skip to main content
. 2017 Sep 6;2017:1256537. doi: 10.1155/2017/1256537

Figure 6.

Figure 6

SEM images of the PLGA_lowT and PLGA_highT plates at different degradation time (0, 15, 30, 60, and 120 days) (bar scale = 1 mm).