. 2017 Sep 20;7:12005. doi: 10.1038/s41598-017-12375-7

Figure 3.

Figure 3

EIS spectra of (a) 10-layered MnO2-deposited electrode, (b) 10-layered RuO2-deposited electrode, and (c) mixed-layered pseudocapacitive electrode composed of 3-layered RuO2 and 2-layered MnO2. VDC = 0 V (vs. Ag/AgCl); amplitude = 10 mV; frequency varies from 100 kHz to 100 mHz; electrolyte = 1 M Na2SO4. Note that open and closed circles denote values obtained before and after stretching the pseudocapacitor yarn, respectively.