Skip to main content
. 2017 Sep 20;7:11932. doi: 10.1038/s41598-017-12296-5

Table 4.

Description of tested solutions. All suppliers confirmed the use of the moist heat method but some did not provide their protocol: A: Not communicated, B: Not communicated, C: F0 ≥ 11, D: F0 ≥ 15 (estimated between at 42 and 45), D’: F0 ≥ 15 (estimated at 20), E: F0 = 15.

Supplier N Conc (%) Volume (ml) Type of Container Type of container material Time-lapse since manufacture (months)
A 20 2.5–5–10 50–100–250–500–1000 Bag PE/PA/PP 7–9–10–12–14–15–16–17–20–31–32–33–34–51
B 15 2.5–5–10–30–50–70 50–100–250–500–1000 Flask – Vial PE - Glass 4–5–6–7–8–11–17–18–25–29–36
C 9 5–10 250–500 Flask – Bag PE – PP 15–16–18–20–34–43–44
D 3 10 250 Bag PP 13–19
D’ 16 5–10–15–30 125–250–500–1000 Vial Glass 10–13–15–18–20–23–25–28–31–33–46–50–54–58–61
E 21 2.5–5–10–15–20–30–50 50–100–250–500–1000 Bag PE/PP - PVC 11–15–16–17–18–20–23–26–29–31–37–41–56