Skip to main content
. 2017 Sep 20;7:12009. doi: 10.1038/s41598-017-12243-4

Figure 5.

Figure 5

(A,B) 2D and (C) 3D AFM and (D) SEM images of the flakes produced after 10s of laser irradiation and deposited on copper.