Mean ± SD (MPa) of compressive strength for all luting cements analysed using Tukey’s test

Luting cement 1 hour 24 hours p value*
RelyXTM U200 138.50 ± 22.8 A 129.20 ± 19.92 A 0.59
Panavia F 110.07 ± 47.5 A 162.33 ± 22.00 A 0.31
G-CEM 153.60 ± 25.15 A 162.60 ± 18.48 A 0.65
CGI Luting 21.36 ± 5.37 B 30.50 ± 22.78 B 0.63

- In each column, mean values with different upper case letters show a significant difference (p value< 0.05).

*

shows significance level of student’s t test between two storage time in each material.