a) Relative bulk and apparent densities, and b) Compressive strength of pure and Fe-doped TCP samples, sintered at 1250 °C, using cylindrical samples (7 mm diameter and 12 mm height). Data is presented as mean ± standard deviation (* P < 0.05 and **P<0.01).