Table 1.

Quantification of the R5 peptide in the GSSR5 composites using FITC labeling technique.

R5 loading Low Medium High
Silk/R5 synthesis ratioa 1/62.5 1/125 1/250
R5 released (%)b 3.8±2.0 3.2±1.4 7.9±3.3
Silk/R5 final ratioc 1/60 1/121 1/205
Encapsulation efficiency (%)d 96.2±2.0 96.8±1.4 92.1±3.3
a

Silk/R5 molar ratio in the GSSR5 composites, determined by the amount of silk and R5 loaded to the composites.

b

The release of the R5 peptide through the process of silicification, determined by

c

quantifying the amount of the FITC-R5 peptide released to the silicifying media. Silk/R5 molar ratio after silicification.

d

Encapsulation efficiencies of the GSSR5 composites