Skip to main content
. 2017 Sep 25;7:12275. doi: 10.1038/s41598-017-12407-2

Figure 1.

Figure 1

(A) The irradiation of an as-deposited nanocrystalline iron thin film to 5 dpa at 300 °C. Note the strong extinction bands, a classic sign of high amounts of strain at a non-equilibrium GB. (B) Irradiation of an annealed film to 5 dpa at 300 °C showing larger dislocation loops.