Skip to main content
. 2017 May 26;8(8):5476–5481. doi: 10.1039/c7sc01514c

Fig. 5. WAXD patterns of the films, annealed at 100 °C for 10 min. Blends 1 and 2, the mixtures of the homochiral polymers having ca. 800 and 1600 repeat units, respectively are compared with l(800)-b-d(800) stereo-diblock copolymer.