The adsorption process at the compaction force of 300KPa, the laying speed of 30 m/min and the pre-heating temperature of 333.15 K: (a) 0 ps; (b) 10 ps; (c) 20 ps; and (d) 30 ps (the arrow refers to the adsorption direction).