Scanning electron micrographs of recycled polystyrene fibers melted at 260 °C at different rotation speeds (A) 6000 rpm; (B) 8000 rpm; (C) 10,000 rpm; (D) 12,000 rpm. Scale bar denotes 100 µm. Arrows denote broken fibers.