Table 11.
Memory shape properties at temperature 45 °C in water bath of materials obtained by Cai et al. [11,31] and materials obtained in this work according to the cycle II.
Properties | PCL/MWCNT/mFe3O4 Composite | PTMG/GNP/mFe3O4 Composite | ||||
---|---|---|---|---|---|---|
CPF3 | PCF50 | PCF100 | MU2 | MU3 | MU4 | |
mFe3O4 content (wt %) | 30 | 30 | 30 | 30 | 30 | 30 |
MWCNT/GNP content (wt %) | 0 | 0.5 | 1 | 0 | 0.5 | 1 |
Time (s) | 26.0 | 13.7 | 13.0 | 12.7 | 6.3 | 10.1 |
Rr (%] | 90 | 95 | 93 | 100 | 99 | 100 |