Skip to main content
. Author manuscript; available in PMC: 2018 Nov 1.
Published in final edited form as: J Mech Behav Biomed Mater. 2017 Jul 13;75:160–168. doi: 10.1016/j.jmbbm.2017.07.017

Fig 10.

Fig 10

Comparison of bending stiffness (N/m), stiffness in compression (N/m) and torsional stiffness (µN·m/°) for all stents. Size of the markers represents radial stiffness scaled down by a factor of 25 for convenience. Torsional stiffness of Supera was 959 µN·m/°.