Skip to main content
. 2017 Oct 4;7:12658. doi: 10.1038/s41598-017-13026-7

Figure 9.

Figure 9

The un-rafted γ′ microstructure of HESA after 800 h creep tests at (a) 750 °C and (b) 850 °C.