Cyclic voltammograms of poly(AHNSA)/GCE in pH 7.0 PBS containing 0.5 mM of SBS at different scan rates (a-l: 10, 20, 40, 60, 80, 100, 125, 150, 200, 250, 350, and 400 mV/s, respectively). Inset: plot of oxidative peak current versus scan rate.