Skip to main content
. 2017 Oct 15;62:91–101. doi: 10.1016/j.actbio.2017.08.045

Fig. 2.

Fig. 2

Representative curves obtained from mercury intrusion porosimetry for PEDOT:PSS scaffolds processed at different temperatures (−26 °C (black curve) or −80 °C (red curve)) and with different crosslinker concentrations (0, 1, 2, or 3 v/v% GOPS). A) Median pore diameter, at a mercury volume intrusion of 50% (dotted lines). B) Pore-diameter distribution. (For interpretation of the references to colour in this figure legend, the reader is referred to the web version of this article.)