Table 2. Initial rates and turn-over frequencies (TOFs) for UiO-67, UiO-67-NMe2, and UiO-67-NH2 .
| MOF | Initial rate (mM s–1) | Half-life (min) | TOFall (s–1) | TOFsurface a (s–1) |
| Full catalyst loading | ||||
| UiO-67 | 0.058 | 4.5 | 0.038 | 5.1 |
| UiO-67-NMe2 | 0.078 | 2 | 0.052 | 7.0 |
| UiO-67-NH2 | 0.067 | 2 | 0.044 | 6.0 |
| Half catalyst loading | ||||
| UiO-67 | 0.018 | 15 | 0.024 | 3.2 |
| UiO-67-NMe2 | 0.049 | 7 | 0.032 | 4.3 |
| UiO-67-NH2 | 0.057 | 3.5 | 0.075 | 10 |
a400 nm particles of UiO-67 are synthesized; as with UiO-66, only the surface sites are expected to be catalytically active.