Skip to main content
. 2017 Oct 20;3(10):eaao0713. doi: 10.1126/sciadv.aao0713

Fig. 1. Schematics illustrating the fabrication process of the 3D Li anode with flowable interphase for solid-state Li battery.

Fig. 1

(A) 3D Li-rGO composite anode was first fabricated. (B) A flowable interphase for the 3D Li-rGO anode was created via thermal infiltration of liquid-like PEG-LiTFSI at a temperature of 150°C. (C) A CPE layer consisting of PEO, LiTFSI, and fumed silica or an LLZTO ceramic membrane was used as the middle layer, and high–mass loading LFP cathode with the CPE as the binder was overlaid to construct the solid-state Li-LFP full cell.