Structural parameter obtained from XRD analysis of ZnO nanoparticles synthesized by milling at different time.

ZnO with different milling hour Lattice parameter in (nm) Tetragonal factor (c/a) Crystallite size (nm)
a c
Bulk (0 h) 0.32495 0.52061 1.602127 50
7 h 0.32426 0.52022 211.604329 22
10 h 0.32414 0.51967 1.603227 18