Table 3.

Carrier concentration, Hall mobility, Hall coefficient, sheet resistance, and optical gap values of the CuxS thin films.

CuxS sample Carrier concentration (×1021 cm−3) Hall mobility (cm2/Vs) Hall coefficient (×10−4 cm3/C) Sheet resistance (×103 Ω) Optical gap (eV)
TF1 2.64 1.18 × 10−2 4.42 1.25 2.07
TF2 1.45 8.64 × 10−3 1.56 1.29 2.50
TF3 2.41 1.96 × 10−3 2.35 7.67 2.28