Figure 5.

Figure 5

Hysteresis of resistance change of brush-painted (a) Ag NW and (b) Ag NW/PEDOT:PSS hybrid electrodes on PU substrate when samples were stretched from 10 to 30%. Inset pictures show stretching steps from 10 to 30%.