Skip to main content
. 2017 Sep 28;7(10):297. doi: 10.3390/nano7100297

Figure 5.

Figure 5

Evolution of weight loss obtained by TGA (a) and DTG (b) of the neat PBAT and PBAT-LDH (5 wt %) nanocomposites (heating rate 20 K·min−1 under nitrogen flow).