. 2017 Oct 12;7(10):315. doi: 10.3390/nano7100315

Figure 1.

Figure 1

Field emission scanning electron microscopy (FE-SEM) images of the surface and cross-section of wet-corroded Ti foil at various temperatures in 5 M KOH aqueous solution: (a,d) 20 °C, (b,e) 50 °C, and (c,f) 80 °C.