Photovoltaic characteristics of wet-corroded Ti foil dye-sensitized solar cells (DSSCs) at 50 °C for different corrosion time periods. IE: ion exchange; FF: fill factor; Voc: open-circuit voltage; η: power conversion efficiency; Jsc: photocurrent density.

Wet Corrosion Time (h) Voc (V) Jsc (mA/cm2) FF (%) η (%)
6 0.63 0.60 72.0 0.27
12 0.64 0.92 71.7 0.42
24 0.67 1.76 68.3 0.80
48 0.69 2.08 71.5 1.03
48 (IE) 0.69 2.28 70.1 1.11