Skip to main content
. 2017 Sep 21;10(10):1110. doi: 10.3390/ma10101110

Figure 7.

Figure 7

Representative XRD patterns of nanofibrous collagen/HA composite microsphere synthesized with different levels of HA: (A) 10 wt %; (B) 15 wt %; (C) 20 wt %, after 3 days of immersion on the SBF solution.