Skip to main content
. 2017 Sep 22;10(10):1124. doi: 10.3390/ma10101124

Figure 13.

Figure 13

Effect of different desorption agents on desorption efficiency of the SLT nanocomposite. (Desorption experiments—sample dosage: 0.05 g; desorption agent concentration: 0.4 mol/L; desorption temperature: 40 °C; desorption time: 30 min).