Skip to main content
. 2017 Oct 3;10(10):1154. doi: 10.3390/ma10101154

Figure 2.

Figure 2

Top view of single layers, and CuKα SEM-EDS maps obtained from the surfaces of LPBF Ti6Al4V (ELI)-1 at % Cu manufactured at laser power of 170 W and 90 µm hatch distance: (a) single scan strategy, scanning speed 0.7 m/s; (b) single scan strategy, scanning speed 1.3 m/s; (c) rescan strategy, scanning speed 0.7 m/s; (d) rescan strategy, scanning speed 1.3 m/s. Some Cu islands pointed out with arrows.