Published in final edited form as: Electrochim Acta. 2017 May 1;235:471–479. doi: 10.1016/j.electacta.2017.03.073

Fig. 5.

Fig. 5

Typical AFM image of Ti3C2Tx (left) and oTi3C2Tx (right) modified Au chip, showing rougher surface of Ti3C2Tx compared to oTi3C2Tx. In both cases z-axis was set to 11 nm.