Skip to main content
. 2017 Oct 29;2017:5839071. doi: 10.1155/2017/5839071

Table 2.

The physicochemical properties between ACECM and WJECM scaffold. Results are reported as mean fold change ± SD from three independent experiments. p < 0.05.

Characteristic ACECM scaffolds WJECM scaffolds
Mean pore size (μm) 193.6 ± 62.1 127.4 ± 42.2
Porosity (%) 75.7 ± 10.5 84.6 ± 3.2
Water swelling ratio 31.1 ± 5.5 16.7 ± 2.3
Compressive modulus (Pa) 297.9 ± 17.9 379.2 ± 28.5