First and peak shock states in experiment S1235.

SS304 Al2024 Permalloy 80 SS304
Pfirst (GPa) 26.9 ± 0.1 15.5 ± 0.1 22.2 ± 0.1 23.0 ± 0.1
Tfirst (°C)  386  142  116 121
Ppeak (GPa) 26.9 ± 0.1 26.9 ± 0.1 23.0 ± 0.1 23.0 ± 0.1
Tpeak (°C)  386  314  235  121

Estimates from successive impedance matches. A 2 mm thick Ta flier launched at 1041 ± 1 ms−1 impacted, in sequence, a 5 mm thick SS304 driver, a 1 mm Al2024 disk, a 1 mm thick permalloy 80 disk, and a 2 cm thick SS304 inner screw.