Figure 2.

Figure 2

pH-induced aggregation-decomposition progress of NaDyF4:10%Nd-GA-Fe. A-C) TEM images of NaDyF4:10%Nd-GA-Fe in aggregation-decomposition progress. D,E) Hydrodiameter vs time plots of NaDyF4:10%Nd-GA-Fe under different pH condition. F) Hydrodiameter vs concentration and pH plots of NaDyF4:10%Nd-GA-Fe. G) Hydordiameter variations of NaDyF4:10%Nd-GA-Fe under the different pH condition for five cycles. These results suggested NaDyF4:10%Nd-GA-Fe can response to different pH condition and hence aggregate in acidic condition.