Figure 3.

Figure 3

IR intensity profiles for heated nozzle, no extrusion, at 230 °C and 100 mm/s. From ROIs corresponding to fig. 1c. The reflection profile is unique for LP, while LP−1 and LP−2 have similar profiles.