Figure 4.

Figure 4

(a) Reflection correction for ABS layer LP−2 printed at 230 °C and 100 mm/s. IR profile from hot extruder w/o extrusion (dashed bluish-green line) shifted to line up with initial peak of extrusion IR intensity (bluish-green). The reflection intensity corresponds to IR profile from the hot extruder w/o extrusion above baseline (black dashed). (b) Time normalized total IR intensives for LP−2 at print speeds of 10 mm/s, 30 mm/s and 100 mm/s.