Published in final edited form as: J Mater Chem B. 2017 May 1;5(22):4137–4151. doi: 10.1039/C7TB00419B

Fig. 5.

Fig. 5

Degradation test on CL-PU(BD), CTC-PU(BD), and CTC-PU(BET) TPU films: (a) weight loss over 10 weeks of degradation, (b) surface morphology of TPUs before and after degradation, and (c) FTIR measurements on TPUs before and after degradation. Scale bars in SEM images are 5 μm.