Skip to main content
. 2017 Nov 6;10(11):1272. doi: 10.3390/ma10111272

Figure 6.

Figure 6

Figure 6

Differences in PANI film surfaces grown on glass substrates when using advanced APPJs device after 60 min deposition without I2 doping, with 30 s I2 doping, and with 120 s I2 doping following deposition: (a) X-ray photoelectron spectroscopy (XPS) survey spectra; and detailed (b) C 1s (high-resolution); (c) N 1s (high-resolution); (d) O 1s; and (e) I 3d spectra. Insets in (a) represent atom percent in PANI film.