Table 2. XPS analysis of the O/C ratio on the surface of UVO-treated plastics after 16 weeks under different storage conditions.
PMMA | COC | PC | |
Air | 0.27 | 0.31 | 0.34 |
Dehumidified | 0.41 | 0.38 | 0.38 |
Vacuum | 0.34 | 0.34 | 0.36 |
PMMA | COC | PC | |
Air | 0.27 | 0.31 | 0.34 |
Dehumidified | 0.41 | 0.38 | 0.38 |
Vacuum | 0.34 | 0.34 | 0.36 |