Table 4. Characterization of NE-AGO kept at different temperature for 1 month.
NE-AGOa | Temperature (°C) |
Size (nm) |
PdI | Zeta potential (mV) | Conductivity (μS/cm) |
---|---|---|---|---|---|
NE-AGO-C | 4 | 204 ± 1.7 | 0.55 ± 0.03 | –38.83 ± 0.92 | 308.3 ± 2.33 |
20 | 144 ± 1.0 | 0.48 ± 0.02 | –21.10 ± 1.14 | 384.0 ± 1.53 | |
40 | 110 ± 1.5 | 0.46 ± 0.01 | –13.30 ± 0.44 | 484.3 ± 2.19 | |
NE-AGO-D | 4 | 78 ± 2.3 | 0.50 ± 0.02 | –25.50 ± 1.15 | 321.0 ± 1.15 |
20 | 66 ± 2.4 | 0.36 ± 0.04 | –27.51 ± 0.45 | 356.0 ± 3.21 | |
40 | 116 ± 1.2 | 0.29 ± 0.01 | –22.37 ± 0.82 | 436.3 ± 2.67 |
Data are presented as means ± S.E.M.
a = NE-AGO-A, NE-AGO-B, NE-AGO-E, and NE-AGO-F were not determined due to phase separation.